家庭裝修時(shí),墻面都需要刮膩?zhàn)樱佔(zhàn)臃鄣姆N類有哪些,加膠水還是加水等相關(guān)問題還是需要注意的。有些朋友擔(dān)心膩?zhàn)臃鄄患幽z水粘不住,有些油漆工會說不加膠水就不會保證墻面質(zhì)量。下面就和福華建材一起來聽聽入行20年的老漆工對于墻面裝修刮膩?zhàn)拥南嚓P(guān)說法。
When family decorates, metope needs to scrape putty, and what kind of putty powder has, add glue or add water and other related problems still need to pay attention to. Some friends worry that putty powder will not stick without glue. Some paint unions say that wall quality will not be guaranteed without glue. The following and Fuhua building materials to listen to 20 years of old painters for wall decoration putty related statements.
一、什么樣的膩?zhàn)臃坌枰幽z水
1、 What kind of putty powder needs glue
傳統(tǒng)非成品膩?zhàn)樱缁邸㈦p飛粉等,它們本身沒有粘性,所以就一定要加膠水。有些油漆師 傅的技術(shù)沒有隨著材料的發(fā)展而進(jìn)步,所以很難掌控膠水配比,擔(dān)心達(dá)不到質(zhì)量標(biāo)準(zhǔn),所以經(jīng)常讓你買輔料。
Traditional non-finished putty, such as talc powder, double fly powder, etc., they have no viscosity, so we must add glue. Some painters' technology does not progress with the development of materials, so it is difficult to control the glue ratio. They are worried that they can not meet the quality standard, so they often ask you to buy accessories.
建筑膠水107和801膠水就經(jīng)常用,價(jià)位便宜,1大桶還不要一百塊。這些膠水里面有級多甲醛,已經(jīng)被停用了。
Building glue 107 and 801 glue are often used, and the price is cheap. It costs less than 100 yuan per barrel. There's a lot of formaldehyde in the glue, which has been stopped.
二、什么膩?zhàn)臃壑灰铀?/div>
2、 What putty powder needs only water
符合國家質(zhì)檢標(biāo)準(zhǔn)的成品膩?zhàn)臃劬筒挥眉幽z!膩?zhàn)臃蹆端谋壤秊?.5:1左右,建議在做墻面施工之前,先涂一層墻固,一定程度上防開裂,提高附著力,讓膩?zhàn)痈玫恼辰Y(jié)在墻上。
Meet the national quality standards of finished putty powder do not need to add glue! The ratio of putty powder to water is about 0.5:1. It is suggested that before the wall construction, a layer of wall cement should be applied to prevent cracking to a certain extent, improve the adhesion, and make the putty stick to the wall better.
三、膩?zhàn)臃凼┕ぷ⒁馐马?xiàng)
3、 Matters needing attention in putty powder construction
墻面一定要批三遍膩?zhàn)?先以找平墻面為準(zhǔn),厚度為0.5mm;再主要用來修補(bǔ)不平整的地方;后是局部找平,所以每一道都不能超過1mm。如果膩?zhàn)庸蔚锰瘢苋菀壮霈F(xiàn)開裂和空鼓的情況。
The wall must be putty for three times, and the first step is to level the wall, with the thickness of 0.5mm; Secondly, it is mainly used to repair the unevenness; After the local leveling, so each should not exceed 1 mm. If the putty is too thick, it is easy to crack and hollow.
墻面如果有開槽、砌墻或不同類型的墻體連接在一起,一定要先掛雙層網(wǎng),再批膩?zhàn)樱@樣能夠減少后期開裂的可能性。
If the walls are slotted, bricked or connected with different types of walls, the double-layer net must be hung first, and then the putty is applied, so as to reduce the possibility of later cracking.